Microsoft Outlookin ja Microsoft 365 -palveluissa on häiriö, joka voi vaikuttaa sähköpostien lähettämiseen ja vastaanottamiseen. Yhteydenottoihimme vastaaminen saattaa viivästyä. Asbesti- ja haitta-ainetutkimusten tilauslomakkeet toimivat normaalisti, ja tutkimustilauksia voi tehdä tavalliseen tapaan. Kiireellisissä asioissa pyydämme soittamaan numeroon 02 282 7780.

Temporary email service disruption

Microsoft Outlook and Microsoft 365 are currently experiencing a service disruption that may affect email delivery and receipt. Our response times may be longer than usual. Our asbestos and hazardous material analysis order forms are working normally, and orders can be submitted as usual. For urgent matters, please call +358 2 282 7780.

Blistering of color coated steel: Use of broad ion beam milling to examine degradation phenomena and coating defects

03.11.2026
← Knowledge Hub

Research publication

Coatings and thin filmsMetals and steelPaper and fibresSample preparationBroad ion beam millingSEM-EDS

Broad ion beam (BIB) cross-section preparation is emerging as a preferred technique to polish delicate multiphase materials. This paper presents an examination of coating degradation phenomena obtained with BIB sample preparation and scanning electron microscopy (SEM) characterization.

Year
2022
Material language
en
Authors / speakers
Ville Saarimaa
Markus Virtanen
Tero Laihinen
Kaisa Laurila
Pasi Väisänen
Journal / publisher
Surface and Coatings Technology

Highlights

  • Broad ion beam polishing is a powerful tool to reveal details in coatings for electron microscopy characterization.
  • BIB cross-section preparation facilitates root cause determination of coating defects.
  • Different development stages of humidity-induced blistering were successfully visualized.

Abstract

Broad ion beam (BIB) cross-section preparation is emerging as a preferred technique to polish delicate multiphase materials. This paper presents an examination of coating degradation phenomena obtained with BIB sample preparation and scanning electron microscopy (SEM) characterization. Early-stage humidity-induced coating degradation included oxidization of zinc and break-up of metal/coating and corrosion inhibitor particle/coating bonding. Ongoing corrosion product formation and accumulation of water within the coating finally led to evolution of macroscopic blisters. These degradation stages were successfully observed from pristine cross-sections, even when blisters did not yet appear on the coating surface, and the technique significantly facilitated distinguishing zinc corrosion-based blistering from other coating defects.

Keywords

  • Organic coatings
  • Zinc
  • Ion beam milling
  • electron microscopy
  • Blistering
  • Delamination

Material and sources

DOI: 10.1016/j.surfcoat.2022.128913

View original resource ↗